The anodic oxidation of platinum

Platinum electrodes were oxidized by means of an " undulant " current. It was found by chemical analysis that the product was practically pure PtO2. HjO ; this was deposited in the anodic, compartment (using i % sulphuric acid as electrolyte) at a rate ot 0-025 g./hr. Details of optimum co...