Comparative study of thermal, mechanical and structural properties of polybutadiene rubber isomers vulcanized using peroxide
Three commercial polybutadiene rubber (BR) compounds (high cis, medium cis and high vinyl content) were vulcanized at 433 K, using different amounts of dicumyl peroxide (DCP) as curing agent. To analyze the structural changes produced by the vulcanization process of the three BR isomers, different e...
Autores principales: | Rodríguez Garraza, A.L., Mansilla, M.A., Depaoli, E.L., Macchi, C., Cerveny, S., Marzocca, A.J., Somoza, A. |
---|---|
Formato: | JOUR |
Materias: | |
Acceso en línea: | http://hdl.handle.net/20.500.12110/paper_01429418_v52_n_p117_RodriguezGarraza |
Aporte de: |
Ejemplares similares
-
Comparative study of thermal, mechanical and structural properties of polybutadiene rubber isomers vulcanized using peroxide
Publicado: (2016) -
Evolution of the free volume and glass transition temperature with the degree of cure of polybutadiene rubbers
por: Mansilla, M.A., et al. -
Evolution of the free volume and glass transition temperature with the degree of cure of polybutadiene rubbers
Publicado: (2013) -
Influence of the crosslinking content on the structural properties of polybutadiene rubbers with different isomeric composition
por: Rodriguez Garraza, A., et al. -
Influence of the crosslinking content on the structural properties of polybutadiene rubbers with different isomeric composition
Publicado: (2016)